Measurement of thermal conductivity and diffusivity of solids, powders, liquids and pastes

Rapid, non-destructive measurement of thermal conductivity and energy efficiency.

The following can be analysed: nanomaterials, explosives, textiles, thermoelectric devices, led systems, rubber, polymers, geological material, insulation, concrete, asphalt, automotive system components.

  • Thermal conductivity measurement range: 0.01 W/(m·K) ÷ 500 W/(m·K),
  • diffusivity measurement range: 0.01 mm²/s ÷ 300 mm²/s,
  • test time: 0.8 s ÷ 5 s,
  • minimum dimension of the test specimen: cylindrical specimen of at least 15 mm in diameter,
  • maximum dimension of the test sample: unlimited,
  • minimum test piece thickness: 0.5 mm, depending on the material's thermal conductivity,
  • maximum thickness of test piece: unlimited,
  • measuring temperature range -50°C ÷ 200°C,
  • measurement according to ASTM D7984.

Device
Model Trident by C-THERM TCi Thermal Conductivity Analyzer (equipped with MTPS,TPS,TLS detectors), by C-Therm Technologies Ltd.